Assab Steel 707 Machinery Steel
Subcategory: Alloy Steel
Close Analogs: AISI 4130, W.nr 1.7218, JIS SCM2
Material Notes: Alloyed machinery steel suitable for weldingApplications: Used for shafts, gears, sprockets, etc., particularly when weldability is required.
|
|
|