Assab Steel STAVAX Supreme Plastic Mold Material
Subcategory: Stainless Steel; Chrome-moly Steel; Metal
Close Analogs: AISI 420 mod
Material Notes: Stainless mould steel with a unique combination of toughness, corrosion resistance and through-hardening properties.Applications: For all type of moulds, especially suited for larger tools where corrosion in production is unacceptable and where high surface finish is required
|
|
|
| Property Data |