Assab Steel EM33 Plastic Mold Material
Subcategory: Alloy Steel
Material Notes: Prehardened plastic mould and holder steel with excellent toughness and machinability.Applications: Plastic and rubber moulds, support plates and constructional parts. Stripper plates in blanking application. Holders/bolsters for plastic moulds and die casting dies.
|
|
|