ATI Wah Chang Niobium
Subcategory: Pure Element; Nonferrous Metal
Material Notes: Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/cc is moderate compared to the majority of the high melting point metals, being less than molybdenum at 10.2 gm/cc and only half that of tantalum at 16.6 gm/cc. Information provided by ATI Wah Chang
| Available Properties |
- Density
- a Lattice Constant
- Covalent Radius
- Electronegativity
- Hardness, Vickers
- Modulus of Elasticity
- Poissons Ratio
- Surface Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Boiling Point
- Brittleness Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|