ATI Wah Chang TI-3Al-2.5V
Subcategory: Titanium Alloy; Nonferrous Metal
Material Notes: Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working and subsequent heat treatment to a wide range of strengths and ductilitys.Information provided by ATI Wah Chang
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Melting Point
- Beta Transus
|
|
|
|