ATI Wah Chang Zircadyne® Alloys Zr 705
Subcategory: Nonferrous Metal; Zirconium Alloy
Key Words: UNS R60705
Material Notes: Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other common engineering alloys.Information provided by ATI Wah Chang
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Shear Modulus
- CTE, linear 68°F
- Melting Point
|
|
|
|
| Property Data |