HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016)
Subcategory: Superalloy; Cobalt Base
Key Words: AMS 5894 MCS 1012 PWA 1196; High Performance Alloys, Inc.
Material Notes: Cobalt content above calculated as remainder. Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of friction, allows sliding contact with other metals without damage by metal pick up in many cases. Seizing and galling can be minimized in applications without lubrication or where lubrication is impractical. Metal seizing is similar to one metal piece building heat against another and they become "welded" together. Galling is when these "weld" areas break off and form an abrasive debris which creates additional abrasion problems. Alloy 6B has outstanding resistance to most types of wear. Its wear resistance is inherent and not the result of cold working, heat treating or any other method. This inherent property reduces the amount of heat treating and post machining. 6B has outstanding resistance to cavitation erosion. Steam turbine erosion shields from 6B have protected the blades of turbines for years of continuous service. 6B has good impact and thermal shock resistance resists heat and oxidation, retains high hardness even at red heat (then cooled, recovers full original hardness) and has resistance to a variety of corrosive media. 6B is useful where both wear and corrosion resistance are needed. Applications: Steam turbine erosion shields, Chain saw guide bars, High temperature bearings, Furnace fan blades, Valve stems, Food processing equipment, Needle valves, Centrifuge liners, Hot extrusion dies, Forming dies, Nozzles, Extruder screws, & many other Misc. wear surfaces. End uses for alloy 6B include half sleeves and half bushings in screw conveyors, tile making machines, rock crushing rollers and cement and steel mill equipment. Alloy 6B is well suited for valve parts, pump plungers. Data provided by High Performance Alloys, Inc.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|