Bales Hard Chrome (QQ-C-320) Mold Coating
Subcategory: Ceramic/Metallic Coating
Material Notes: Description: Hard Chrome provides excellent wear resistance to glass filled resins. It can be selectively plated up to .020 for shims and inside or outside diameter corrections that need E.D.M. or grinding to finished size. Hard Chrome is a great way to save precision pieces that cannot be welded.Information provided by Bales Mold Service Inc.
| Available Properties |
- Hardness, Rockwell C
- Coefficient of Friction
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|