Bales Nicklon® (Nickel-P.T.F.E.) Mold Coating
Subcategory: Metal Matrix Composite; Nickel Alloy; Ceramic/Metallic Coating
Material Notes: Description: Autocatalytic application provides a uniform layer of 22%-24% PTFE over the deepest ribs and most complex details. It is also corrosion resistant.Excellent Release Properties for: - Deep Ribs
- "No Draft" Cores
- Textured Surfaces
- Difficult to Eject Polymers
Information provided by Bales Mold Service Inc.
| Available Properties |
- Hardness, Rockwell C
- Coefficient of Friction
- Processing Temperature
|
|
|
|