Bales Sulfamate Nickel (QQ-N-290) Mold Coating
Subcategory: Nickel Alloy; Ceramic/Metallic Coating
Material Notes: Description: Selective plating for dimensional correction is a typical application for Sulfamate Nickel because of it's ability to deposit up to .250 with less inclusions and porosity than most electrolytic deposits. This is an excellent choice for deposits in excess of .015-.020 thick.Information provided by Bales Molding Service Inc.