Brush Wellman BrushBronze™ 95510 (AMS 4880) Centrifugal Cast 0.250" - 1.0"
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: UNS C95510
Material Notes: Information supplied by Brush Wellman Engineered Materials. BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under severe loading conditions. This material, specified as AMS 4880, is frequently used for very demanding aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. This material is also commonly used for applications in the oil and gas and other durable goods markets. BrushBronze™ 95510 (AMS 4880) offers several significant advantages over other materials available in the marketplace due to the EquaCast™ process:
- Higher and more consistent mechanical properties
- Improved service life
- Superior quality
- Ease of use
- Cost effectiveness
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|