Brush Wellman BrushBronze™ 630 (AMS 4640) 0.250" - 1.0"

 

Subcategory: Copper Alloy; Nonferrous Metal; Bronze

Material Notes:
Information supplied by Brush Wellman Engineered Materials.

BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading conditions. This material, specified as AMS 4640, is frequently used for very demanding aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. This material is also commonly used for applications in the oil and gas and other durable goods markets.

BrushBronze™ 630 (AMS 4640) offers several significant advantages over other materials available in the marketplace due to the EquaCast™ process:

  • Higher and more consistent mechanical properties
  • Improved service life
  • Ease of use

Available Properties
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。