Brush Wellman Brush 60™ HT

 

Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy

Key Words: UNS C17460

Material Notes:
Copper content calculated as remainder. Information supplied by Brush Wellman Engineered Materials.

Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%
Stress Relaxation after 1000 hrs @ 200°C: 75%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.5
Formability Ratio (bad Way): 1.5
Superficial Hardness: 30T 82-89

Brush 60™ is a new generation, high conductivity copper beryllium alloy which is specifically engineered to meet the stringent electrical and mechanical requirements of computer, datacom, and telecommunications applications. Performance benefits include:

  • Signal reliability
  • Durability
  • Design flexibility
  • Manufacturability
  • Recyclability

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。