Brush Wellman Beryllium Copper Alloy 165 Strip; HT (TH04) Temper (UNS C17000)
Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy
Close Analogs: This material has been discontinued.
Key Words: ASTM B-194, QQ-C-533
Material Notes: Copper content above calculated as remainder. Treatment required for max strength: 2 hrs @ 315ºC Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98% Stress Relaxation after 1000 hrs @ 200°C: 75% Superficial Hardness: 30N 58-63 Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.
| Available Properties |
- Density
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|