Brush Wellman Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; up to 76 mm o.d. (UNS C17200)
Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy
Key Words: RWMA Class 4, ASTM B-643, AMS 4535
Material Notes: Copper content above calculated as remainder. Treatment required for max strength: 3 hrs @ 315-330°C or Mill Hardened Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|