Brush Wellman ToughMet® AT Temper T3 AT90(OD≥4")
Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal
Material Notes: Description: ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engineered ToughMet® to provide attributes beyond those typically found in a high-strength copper alloy.- Exceptional resistance to corrosion and cavitation
- Outstanding lubricity and durability in demanding applications
- Highly uniform composition in all product forms
- Uniform microstructure in a variety of wrought shapes and sizes
ToughMet® 3 in the wrought and spinodally hardened (AT) condition exhibits tensile strength up to 140 ksi and hardness up to HRc 34 in a Copper-15% Nickel-8% Tin alloy with excellent machinability. Copper content calculated as remainder. Information supplied by Brush Wellman Engineered Materials.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|