Brush Wellman ToughMet® CX Temper T3 CA

 

Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal

Material Notes:
Description: ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engineered ToughMet® to provide attributes beyond those typically found in a high-strength copper alloy.

  • Exceptional resistance to corrosion and cavitation
  • Outstanding lubricity and durability in demanding applications
  • Highly uniform composition in all product forms
  • Uniform microstructure in a variety of wrought shapes and sizes

ToughMet® 3 in the cast and spinodally hardened (CX) condition exhibits tensile strength up to 120 ksi and hardness up to HRc 34 in a Copper-15% Nickel-8% Tin alloy with excellent machinability.

Copper content calculated as remainder. Information supplied by Brush Wellman Engineered Materials.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 68°F
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。