Brush Wellman PROtherm® Beryllium Copper Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy
Material Notes: Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a unique combination of thermal conductivity and strength, which allow for :- Shorter cycle times and reduced part costs
- Improved part quality leading to a substantially lower scrap rate
- 3 times faster machining rates resulting in lower cost molds and shorter delivery times
- Processing that is similar to tool steels with no substantial processing changes required
- One million + cycles leading to lower maintenance costs
- A reduction in cost for Moldmakers
- Reduced cost and high part quality at a lower piece price for Molders
PROtherm® provides the highest thermal conductivity available in a mold material… ten times greater than steel and twice that of aluminum. PROtherm® also offers a hardness and strength that exceeds aluminum. PROtherm® is specifically designed for foam processing; core caps, hot runner systems and other applications where maximum heat removal or control are required. Information supplied by Brush Wellman Engineered Materials.
| Available Properties |
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Elongation at Yield
- Compressive Yield Strength
- Charpy Impact
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|