Brush Wellman BrushCAST® 275CT Fine Grain Casting Alloy (As Cast)
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: UNS C82800
Material Notes: Copper content above calculated as remainder. Pouring Temperature: 960-1035°C Heat treatment required for max strength (Annealing): 760-790°C/water quench Heat treatment required for max strength (Hardening): 760-790°C/water quench Description: The unique combination of physical and mechanical properties of copper beryllium casting alloys provide a dynamic range of metallurgical alternatives to meet specific performance requirements. The inherent strength, hardness, conductivity, and castability of these materials make them ideal for applications which require a high performance engineered material solution. Advancements in component casting technology and proprietary material production technology pioneered by Brush Wellman have resulted in BrushCAST™ alloys being a cost effective design choice. BrushCAST™ high strength casting alloys are available in fine grain equivalents. Material properties and manufacturing characteristics are similar to those of the standard casting alloys. Grain refinement is achieved through precise additions of either cobalt or titanium. Our fine grain casting alloys are preferred in applications where excellent surface finish characteristics are required in the cast product. Information supplied by Brush Wellman Engineered Materials.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|