Bethlehem Steel ASTM A242-87 TYPE 1 (MAYARI-R), >1-1/2 to 4 in. thick, steel plate
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: Data published in 1997. Bethlehem Steel in no longer in business.
Material Notes: A242 is a high-strength, low-alloy grade that has 4 times the corrosion resistance of carbon steels without copper. It is a corrosion-resistant steel whose oxide forms a protective coating. Used in many painted and unpainted applications (buildings, bridges, industrial equipment, railroad rolling stock, etc.)Information provided by Bethlehem Steel Corporation
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|