MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Bethlehem Steel ASTM A514 Grade P, 1/4 to 2-1/2 in. thick, steel plate

 

Subcategory: ASTM Steel; Low Alloy Steel; Low Carbon Steel; Metal

Close Analogs: Data published in 1997. Bethlehem Steel in no longer in business.

Material Notes:
A514 is an alloy steel grade, fully killed, fine grain. It is heat treated by quenching and tempering. The specification permits 18 compositions, of which Bethlehem produces Grades B, H and P. Its normal uses are industrial applications where high strength, low weight and high impact values are required. Machinery, mining equipment and other demanding applications.

The following are suggested consumables for arc welding processes for 0.476 - 6.35 cm (3/16 - 2.5 in.) thicknesses: For Manual Shielded Metal-Arc (AWS A5.5) use Low Hydrogen Electrodes E11015, E11016, and E11018. For Submerged Arc (AWS A5.23) use F11x-Exxx. For Gas Metal-Arc (AWS A5.28) use ER110S. For Flux Cored-Arc (AWS A5.29) use E11xT.

Information provided by Bethlehem Steel Corporation

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Bend Radius, Minimum
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。