Bethlehem Steel ASTM A529 Grade 42, 3/16 to 1/2 in. thick, as-rolled steel plate
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: Data published in 1997. Bethlehem Steel in no longer in business.
Material Notes: A low cost grade limited to 1/2 inch thickness, used occasionally for non-demanding applications.The following are suggested consumables for arc welding processes for 0.476 - 1.27 cm (3/16 - 1/2 in.) thicknesses. For Manual Shielded Metal-Arc (AWS A5.5) use Low Hydrogen Electrodes E60xx, and E70xx. For Submerged Arc (AWS A5.23) use F6x-Exxx, and F7x-Exxx. For Gas Metal-Arc (AWS A5.28) use ER70S-x. For Flux Cored-Arc (AWS A5.29) use E6xT-x, and E7xT-x except -2, -3, -10, or -GS. Information provided by Bethlehem Steel Corporation
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|