Bethlehem Steel ASTM A633 Grade A, 3/16 to 2-1/2 in. thick, steel plate
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Close Analogs: Data published in 1997. Bethlehem Steel in no longer in business.
Material Notes: Particularly well suited for low-temperature use where notch toughness is a requirement and when strength/weight ratios must me maximum for the application.Information provided by Bethlehem Steel Corporation
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|