Bisalloy Steels BisPlate 60, >80-100 mm
Subcategory: Low Alloy Steel; Low Carbon Steel
Key Words: ASTM A537 Class 2, ASTM A572 Grades 60 & 65, JIS G3106 SM570, ISO 4950-3 E460, BS 4360 Grade 55F, ISO 9328-4 P460 & P500 grade
Material Notes: Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment Testing: AS/NZS 3597 Grade 500 NATA approved Welding: According to AS/NZS 1554 parts 4 and 5 Tolerance: In accordance with AS/NZS 1365
| Available Properties |
- Hardness, Brinell
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- CE (IIW)
- PCM
- Surface Finish
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|