Bisalloy Steels BisPlate 80, =16-80 mm
Subcategory: Low Alloy Steel; Low Carbon Steel
Key Words: ASTM A514, ISO 4950-3 Grade E690, ISO 9328-4 Grade P690TQ, EN 10137-2 Grade S690Q, JIS G3128
Material Notes: Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the high strength properties of BISPLATE 80 allows reduction in section thickness without loss of structural integrity.Applications: Transport Equipment, High Rise Buildings, Bridges, Excavator Buckets, Storage Tanks, Lifting Equipment, Mining Equipment, Induced Draft Fans Testing: AS/NZS 3597 Grade 700 NATA approved Welding: According to AS/NZS 1554 parts 4 and 5 Tolerance: In accordance with AS/NZS 1365
| Available Properties |
- Hardness, Brinell
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- CE (IIW)
- PCM
- Surface Finish
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|