Bisalloy Steels BisPlate 450, 8-20 mm
Subcategory: Low Alloy Steel; Low Carbon Steel
Material Notes: A through hardened, abrasian resistant steel plate, with guaranteed high impact toughnessApplications: Dump Truck Bodies, Mining Buckets, Tipper Bodies, Cutting Edges, Dump Truck Wear Liners, Construction Waste Bins, Liner Plates/Chutes Testing: AS/NZS 1816, AS/NZS 1544 Tolerance: In accordance with AS/NZS 1365
| Available Properties |
- Hardness, Brinell
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- CE (IIW)
- CET
- Surface Finish
|
|
|
|
| Property Data |