Bisalloy Steels BisPlate 80PV, =16-80 mm
Subcategory: Low Alloy Steel; Low Carbon Steel; Metal
Key Words: ASTM A517, EN 10028-6 Grade P690Q
Material Notes: A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage Tanks, Railroad Tankers, Refinery and Petro Chemical Equipment Testing: AS/NZS 3597 Grade 700PV NATA approved Welding: According to AS/NZS 1554 parts 4 and 5 Tolerance: In accordance with AS/NZS 1365
| Available Properties |
- Hardness, Brinell
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- CE (IIW)
- PCM
- Surface Finish
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|