UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal
Material Notes: Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in order to give mechanical properties with maximum isotropy and is certified to meet a minimum Charpy V-notch test result of 10 ft-lbs (13.6 J). Suitable for a wide variety of hot work applications, including tools for high pressure die casting, hot extrusion and press forging, Orvar® Superior meets or exceeds the NADCA 207-97 and the 207-2003 Superior Specification in dimensions up to 18” in thickness. Orvar Superior is characterized by: - A high level of resistance to thermal shock and thermal fatigue
- Good high-temperature strength
- Excellent toughness and ductility in all directions
- Good machinability and polishability
- Excellent through-hardening properties
- Good dimensional stability during hardening
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Charpy Impact
- CTE, linear, 482°F (250°C)
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|