UDDEHOLM HOTVAR® Hot Work Tool Steel
Subcategory: Tool Steel; Hot Work Steel; Alloy Steel; Metal
Material Notes: Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are balanced to give high hot wear resistance and good high temperature properties. Manufactured by special techniques, Hotvar® is suitable for applications where hot wear and/or plastic deformation are the dominating failure mechanisms. Hotvar is characterized by: - High hot wear resistance
- Very good high temperature properties
- High resistance to thermal fatigue
- Very good temper resistance
- Very good thermal conductivity
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Charpy Impact
- CTE, linear, 482°F (250°C)
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|