UDDEHOLM IMPAX® SUPREME (Modified AISI P20) Hot Work Tool Steel
Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal
Material Notes: Chromium-nickel-molybdenum alloyed steelA pre-hardened Ni-Cr-Mo-steel supplied at 290-341 HB suitable for die casting of zinc, lead and tin. Also suitable for high strength holder blocks. Impax Supreme offers the following benefits: - No hardening risks
- No hardening costs
- Time saving, e.g. no waiting for heat treatment
- Lower tool cost
- Modifications easily carried out
- Can be subsequently nitrated to increase surface wear resistance or locally flame hardened to reduce surface damage
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- Charpy Impact
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|