UDDEHOLM ALVAR 14 Hot Work Tool Steel
Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal
Key Words: W.Nr. 1.2714; NiCrMoV7
Material Notes: Chromium-nickel-molybdenum-vanadium alloyed steelALVAR 14 is recommended for support tooling in extrusion (e.g. bolsters and wedge blocks). This material is available mill direct. ALVAR 14 is characterized by: - Good toughness
- Excellent resistance to high thermal stresses
- Excellent stability in hardening
- Excellent through-hardening properties
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- CTE, linear, 482°F (250°C)
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|