UDDEHOLM VANADIS 23® (AISI M3:2) Hot Work Tool Steel
Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal
Material Notes: Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications where wear resistance above that of an ORVAR 2M / AISI H13 is required. This material is available in limited sizes. Vanadis 23 is characterized by: - High wear resistance (abrasive profile)
- High compressive strength
- Very good through-hardening properties
- Good toughness
- Very good dimensional stability on heat treatment
- Very good temper resistance
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Flexural Strength
- Flexural Yield Strength
- Impact Test
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Shrinkage
- Deflection, mm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|