BOHLER W302 SUPERIOR® (Premium AISI H13) Hot Work Tool Steel
Subcategory: Tool Steel; Hot Work Steel; Alloy Steel; Metal
Key Words: DIN 1.2344; JIS SKD61; 40CrMoV5
Material Notes:
This premium H13 grade steel, produced via special melting and refining techniques possesses excellent toughness making it suitable for demanding hot work applications. W302 Superior meets or exceeds NADCA 207-97 and 207-2003 Superior Specification in dimensions 18" and greater in thickness. A premium grade H13 hot work tool steel featuring: - Very good toughness properties
- Very good heat checking resistance
- Good temper resistance and high temperature strength
- Excellent polishability and texturability
- Manufactured for flats greater than 18 inches in thickness
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Electrical Resistivity
- CTE, linear, 212°F (100°C)
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|