UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Subcategory: Tool Steel; Alloy Steel; Metal
Material Notes: Chromium-molybdenum-vanadium alloyed steelSuitable for long run tooling where adhesive wear is dominant and/or the risk of chipping or cracking is very high, e.g. blanking, fine blanking and forming of thicker work material such as austenitic stainless steel, mild carbon steels, UHSS, copper and aluminum. Also used for granulator knives and cold forging applications. Vanadis 4 Extra is characterized by: - Very good ductility
- High abrasive-adhesive wear resistance
- High compressive strength
- Good dimensional stability during heat treatment and in service
- Very good through hardening properties
- Good temper back resistance
- Good machinability and grindability
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Impact Test
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|