UDDEHOLM VANADIS 10® SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
Subcategory: Tool Steel; Cold Work Steel; Alloy Steel; Metal
Material Notes: Chromium-molybdenum-vanadium alloyed steelSuitable for very long run tooling where abrasive wear is dominant, e.g. blanking and forming of abrasive material, blanking of electrical sheet steel, blanking of gaskets, paper and foil slitting, granulator knives, extruder screws, etc. Vanadis 10 is characterized by: - Extremely high abrasive wear resistance
- High compressive strength
- Very good through hardening properties
- Good toughness
- Very good stability in hardening
- Good resistance to tempering back
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Impact Test
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Pin-On-Disc wear
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|