General Grade AISI O1 Cold Work Tool Steel
Subcategory: Tool Steel; Cold Work Steel; Alloy Steel; Metal
Key Words: AISI O1, W.-Nr. 1.2510
Material Notes: Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface hardness and toughness after hardening and tempering. AISI O1 is characterized by: - Good machinability
- Good dimensional stability in hardening
- A good combination of high surface hardness and toughness after hardening and tempering
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|