General Grade AISI A2 Cold Work Tool Steel
Subcategory: Tool Steel; Cold Work Steel; Alloy Steel; Metal
Key Words: AISI A2; W.-Nr. 1.2363
Material Notes: Chromium-molybdenum-vanadium alloyed steelSuitable for medium run tooling. This grade features good machinability, high stability after hardening and good wear resistance. AISI A2 can be supplied in various finishes, including the hot-rolled, pre-machined and fine-machined condition. It is also available in the form of hollow bar and rings. AISI A2 is characterized by: - Good machinability
- High stability after hardening
- High compressive strength
- Good hardenability
- Good wear resistance
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|