General Grade AISI D2 Cold Work Tool Steel
Subcategory: Tool Steel; Cold Work Steel; Alloy Steel; Metal
Key Words: AISI D2; W.-Nr. 1.2379
Material Notes: Chromium-molybdenum-vanadium alloyed steelAISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadium. Suitable for medium run tooling for applications where abrasive wear is dominant and the risk of chipping or cracking is not so high, e.g. for blanking and forming of thinner, harder work materials. AISI AD2 is characterized by: - High wear resistance
- High compressive strength
- Good through-hardening properties
- High stability in hardening
- Good resistance to tempering-back
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- CTE, linear, 212°F (100°C)
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|