UDDEHOLM RAMAX® S Modified 420F
Subcategory: Stainless Steel; Chrome-moly Steel; Alloy Steel; Metal
Key Words: AISI 420F
Material Notes: Chromium alloyed stainless holder steelA pre-hardened stainless holder steel with excellent machinability, high tensile strength and good corrosion resistance. RAMAX® S is characterized by: - Excellent machinability
- Good corrosion resistance
- Uniform hardness in all directions
- Good indentation resistance
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Impact Test
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|