Brush Wellman, Inc. PROtherm® Beryllium Copper Mold Material
Subcategory: Copper Alloy; Beryllium Alloy
Material Notes:
A high conductivity beryllium copper mold alloy. For applications requiring very high thermal conductivity but with moderate strength and wear demands. PROtherm® is characterized by: - Extremely high thermal conductivity
- Excellent corrosion resistance
- Good polishability and machinability
- Good resistance to galling
- Excellent weldability
- Rapid, uniform heat transfer
- Resistance to high temperature (e.g. for engineering thermoplastics)
- Ability to be coated for higher wear resistance
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|