Brush Wellman, Inc. moldMAX® XL High Strength Copper Alloy
Subcategory: Copper Alloy
Material Notes:
moldMAX® XL is characterized by: - High thermal conductivity
- Excellent machinability
- Good polishability and
- Good corrosion resistance
- Good wear resistance
- High impact strength
- Excellent resistance to galling
- Large cross sectional availability
Information provided by Bohler-Uddeholm
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|