BOHLER M300 Modified 420

 

Subcategory: Stainless Steel; Alloy Steel; Metal

Key Words: DIN 1.2316; DIN X36CrMo17; EN X38CrMo16

Material Notes:
Stainless martensitic chromium steel

BOHLER M300 is ideal for applications such as plastic extrusion dies and cores and cavities for injection molding. BOHLER M300 can be supplied in both the pre-hardened and annealed conditions.

BOHLER M300 is a stainless steel with elevated chromium content for resistance to corrosive environments and high cleanliness levels for applications requiring highly polished surfaces.

Information provided by Bohler-Uddeholm

Available Properties
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。