Cadi Company Cadi 162 Copper Alloy
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: UNS C16200
Material Notes: Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium Copper is also specified for spot welding aluminum; the high thermal conductivity helps to prevent electrode sticking on these soft, conductive materials. Forms: Information provided by Cadi Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Processing Temperature
- RMWA Class
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|