Cadi Company Cu-Tungsten (75%) Copper Alloy
Subcategory: Metal Matrix Composite; Copper Alloy; Tungsten Alloy; Nonferrous Metal; Refractory Metal
Key Words: ASTM B702
Material Notes: For projection welding electrodes where pressures are moderately high. This grade is the standard for many copper tungsten resistance welding applications. Information provided by Cadi Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Electrical Resistivity
- RMWA Class
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|