Cadi Company Cu-Tungsten (80%) Copper Alloy
Subcategory: Metal Matrix Composite; Copper Alloy; Tungsten Alloy; Nonferrous Metal; Refractory Metal
Key Words: ASTM B702
Material Notes: Slightly higher tungsten content results in higher hardness and strength when forces are relatively high. Strength is gained with a slight decrease in electrical and thermal properties. Information provided by Cadi Company.