Copper Clad 1006 Steel (40% Conductivity)
Subcategory: Nonferrous Metal
Material Notes: All values may vary dependant on specific design and usage 1006 steel core, 99.99% copper clad Capabilities: - Wire
- Ribbon
- Square
- Insulated
- Plated
Information provided by California Fine Wire.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Electrical Resistivity
- Maximum Service Temperature, Air
- Magnetic
|
|
|
|