Gall-Tough® Stainless
Subcategory: Stainless Steel; T S20000 Series Stainless Steel; Metal
Key Words: ASTM A479; ASTM A276; ASTM A314; ASTM A580; ASTM A240, Stainless Steel; Carpenter Technology Corporation, Carpenter Steel Division; Cartech
Material Notes: Iron content calculated as remainder. Data provided by Carpenter Technology Corporation. 6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground. Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm. Gall-Tough® stainless is a high silicon, high manganese, nitrogen strengthened, austenitic stainless alloy which possesses superior self-mated galling resistance and metal-to-metal wear resistance. The alloy possesses higher strength and high temperature oxidation resistance than Type 304 stainless with comparable corrosion resistance, depending on the environment. Gall-Tough® is a registered trademark of Carpenter Technology Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|