|   BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr  Subcategory: Superalloy; Nonferrous Metal; Cobalt Base Key Words: ASTM F799; ASTM F1537; ISO 5832-4; ISO 5832-12 Material Notes: Cobalt content calculated as remainder.  Data provided by Carpenter Technology Corporation.
 Annealing followed by water quench and low stress grinding prior to tensile testing. Medical Implant Alloy.  Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance.  BioDur CCM Plus alloy is a wrought powder metallurgy product produced by vacuum induction melting (VIM) followed by inert gas atomization and hot isostatic pressing to produce 100% dense billets.  These billets are then processed by conventional steel-making practices to make finished products. Biodur™ and CCM Plus™ are trademarks of Carpenter Technology Corporation. 
| | 
    | Available Properties |  
    | DensityHardness, BrinellHardness, KnoopHardness, Rockwell CHardness, VickersTensile Strength, UltimateTensile Strength, YieldElongation at BreakReduction of AreaCTE, linear 20°CCTE, linear 250°CCTE, linear 500°CCTE, linear 1000°CSpecific Heat CapacityThermal Conductivity
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |