Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC

 

Subcategory: Superalloy; Nonferrous Metal; Nickel Base

Key Words: UNS N07716; NACE MR0175; ASTM B805; AMS 5854

Material Notes:
Iron content calculated as remainder. Data provided by Carpenter Technology Corporation.

Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to that of Alloy 625 and superior to that of Alloy 718. A yield strength (0.2% offset) above 120 ksi (827 MPa) can be obtained by aging without prior warm or cold working. The precipitation hardening capability is particularly important in applications where large-section size or intricate shape precludes warm working. In the age hardened (high strength) condition, Custom Age 625 PLUS alloy offers exceptional resistance to stress corrosion cracking as well as general, pitting and crevice corrosion.

Custom Age 625 PLUS alloy could be considered for applications where severely corrosive environments are a concern, such as those encountered in deep sour gas wells as well as in a variety of refinery and chemical process industry applications. In addition, Custom Age 625 PLUS alloy could be considered a candidate for use in marine environments, where Alloy 625 has been used successfully. The higher strength capability of Custom Age 625 PLUS alloy may be particularly useful for fasteners and shafts. fexxxData provided by Carpenter Technology Corporation.

Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to that of Alloy 625 and superior to that of Alloy 718. A yield strength (0.2% offset) above 120 ksi (827 MPa) can be obtained by aging without prior warm or cold working. The precipitation hardening capability is particularly important in applications where large-section size or intricate shape precludes warm working. In the age hardened (high strength) condition, Custom Age 625 PLUS alloy offers exceptional resistance to stress corrosion cracking as well as general, pitting and crevice corrosion.

Custom Age 625 PLUS alloy could be considered for applications where severely corrosive environments are a concern, such as those encountered in deep sour gas wells as well as in a variety of refinery and chemical process industry applications. In addition, Custom Age 625 PLUS alloy could be considered a candidate for use in marine environments, where Alloy 625 has been used successfully. The higher strength capability of Custom Age 625 PLUS alloy may be particularly useful for fasteners and shafts.

Custom Age 625 PLUS® is a registered trademark of Carpenter Technology Corporation.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。