Carpenter Pyromet® Alloy CTX-3 Superalloy, Heat Treated
Subcategory: Superalloy; Iron Base
Key Words: Pyromet Alloy 907, Carpenter Technology Corporation, Carpenter Steel Division; Cartech
Material Notes: Iron content calculated as remainder. Data provided by Carpenter Technology Corporation. Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy also possess high hot hardness and good thermal fatigue resistance. It is weldable, brazable, and can be chromium plated. This material offers significant improvement in notched stress-rupture strength over Pyromet alloy CTX-1. Retained hot-cold work is not required for good stress rupture properties and is not affected by stress orientation. Pyromet® is a registered trademark of Carpenter Technology Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|